Contact SupplierWe are offering rolling mild steel bars from sizes from 28 mm to 125 mm.
We have in-house facilities like rolling, annealing, straightening and facility for bright bar (draw, pilling, centralized grinding) production. This is also supported by our lab facilities like spectrometer, mpi, hardness testing, uts etc.
Our rolling mill has capacity of 50,000 tonsyear and we are already in process of setup of a new mill. After that we can roll small bars and structural's. We are also doing conversion for reputed alloy steel producers and have additional capacity available for doing more conversion work.
We are regularly making the following steel grades:
ms, en-19sae-4140, en-24, en-31sae-5200, 20mncr5, en1a, en-8d, en-9, ss etc.