Our Products
We are a notable Manufacturer, Exporter and Supplier of Cold Face Insulation Bricks. Cold Face Insulation Bricks find their usage in the areas requiring no thermal and electrical degradation. We manufacture these Cold Face Insulation Bricks at par with the industry standards. They are extensively demanded by the clients.
Specialties :Test Report
s. n. | Bd. (gm/c) | c.c.s. (gm/cm2) | AP % | P.L.C ( (1000 C2 Hrs)) |
T.C. (Kcal/Cm2/Hr/c) |
---|---|---|---|---|---|
1 | 0.75 | 15.2 | 70.2 | - | - |
2 | 0.77 | - | 72.4 | + - 0.80 | - |
3 | 0.79 | 13.5 | 71.5 | - | 0.144 |
4 | 0.80 | - | 70.6 | + - 0.82 | - |
5 | 0.76 | 14.6 | 71.4 | - | 0.148 |
We are engaged in manufacturing, supplying and exporting of Arch Fire Bricks. Arch Fire Bricks are used for bigger openings of furnace roofs. We provide the different types of Arch Fire Bricks to the clients such as Side Arch Bricks/Side Taper Bricks and End Arch Bricks/End Taper Bricks. We make Arch Fire Bricks available at economical rates.
Attributes :Length-L | Breadth/Width-B | Thickness-T | |
T-1 | T-2 | ||
228mm 9" | 114mm 4-" | 75mm 3" | 70mm 2-" |
228mm 9" | 114mm 4-" | 75mm 3" | 65mm 2-" |
228mm 9" | 114mm 4-" | 75mm 3" | 65mm 2-" |
228mm 9" | 114mm 4-" | 75mm 3" | 50mm 2" |
228mm 9" | 114mm 4-" | 75mm 3" | 38mm 1-" |
250mm 10" | 123mm 5" | 73mm 2" | 65mm 2" |
250mm 10" | 123mm 5" | 70mm 2" | 60mm 2" |
250mm 10" | 123mm 5" | 73mm 2" | 57mm 2" |
We are one of the renowned Hot Face Insulation Bricks Manufacturers, Exporters and Suppliers. These Hot Face Insulation Bricks are used in boilers, furnaces, etc. for heat insulation. We make these Hot Face Insulation Bricks available at fairly economical prices.
Specialties :Specifications
Properties | SIPL-7 | SIPL-8 | SIPL-9 | SIPL-l0 | SIPL-13 | SIPL-14 | SIPL-15 |
---|---|---|---|---|---|---|---|
Service Temperature inoC | 1050 | 1200 | 1250 | 1250 | 1300 | 1400 | 1500 |
Bulk Density in gms/cc (Max) | 0.8 | 0.85 | 0.9 | 1.0 | 1.1 | 1.2 | 1.3 |
Apparent Porosity in % (min) | 70 | 65 | 60 | 60 | 55 | 50 | 50 |
Cold Crushing strength in kg/cm2/(min) | 12 | 15 | 20 | 25 | 30 | 30 | 40 |
Thermal Conductivity in KcaI/M/Hr/oC(Max)at Hot face temperature of 600oC (max) | 0.20 | 0.23 | 0.26 | 0.28 | 0.30 | 0.35 | 0.40 |
Paramanent Linear change after re-heating (max) in % | 1.5 | 1.5 | 1.5 | 1.5 | 1.5 | 1.5 | 1.5 |
for 3 hrs at temperature of | 1050 | 1200 | 1250 | 1250 | 1300 | 1350 | 1450 |
Test Report
S.No. | B.D. (gm/c) | C.C.S. (gm/cm2) | AP% | P.L.C. (1000 c 2 Hrs) | T.C. (Kcal/Cm2/Hr/c) |
---|---|---|---|---|---|
1 | 0.88 | 24.8 | 65.7 | + - 0.78 | - |
2 | 0.85 | 22.2 | 67.5 | - | 0.123 |
3 | 0.87 | 23.1 | 68.2 | + - 0.72 | - |
4 | 0.89 | 26.6 | 66.4 | - | 0.134 |