Our Products
Coat I:
Primer Coat: Mixture of grey cement and acrylic polymer with fine sand and PPF to be brushed.
Coat II:
White Coat: Titanium mixed with Roof Tiles White Powder, acrylic polymer, fine sand and PPF to be brushed on Primer Coat.
Coat III:
White Coat: Titanium mixed with Roof Tiles White Powder, acrylic polymer, fine sand and PPF to be brushed on second coat.
Coat IV:
Final protective coat of Roof Tiles Nano White to be applied on white coat.
Specifications are subject to change for improvement without any prior information.
Parameters | Roof Tiles White Tiles | Roof Tiles White Coat |
---|---|---|
Excepted Life under normal conditions | 50 years | 5 years |
Installation Cost with limited warranty | Rs 100 per sq ft | Rs 35 per sq ft |
Cool Roof requirements as per ECBC norms: (Reflective tiles or Heat Resistant tiles) (ASTM E 1980-11, EN 673:2011 and EN 410:2011) |
Roof Tiles Value | How much weathering course is required for cool roof? | |||
---|---|---|---|---|---|
Solar Reflectance Index |
>78 |
96 |
A building receives most of the heat through roof by radiation. Heat moves in and out of your home (or about any other structure) in four ways: by conduction (which R-Value measures), and by convection, radiation (which S.R.I value measures) and air infiltration. |
||
Solar Direct Reflectance |
0.70 |
0.77 |
|||
Emissivity |
0.75 |
0.92 |
|||
Energy Conservation Building Code (section 4.3.1 & 4.3.1.1) |
Sl.No: | PARAMETER | METHOD /STDs | Roof Tiles VALUE | REMARKS |
1) | Dimension | - | 300x300x9.0 mm | |
2) | Weight per Sq ft | - | 1.25 to 1.30 kg | |
5) | Scratch Hardness (Moh's) | IS 13630 (part 13) | >6 (6 to 7 for vitrified tile) | Unique property of Roof Tiles Cool Roof |
7) | Accelerated Weathering Test | IS 101 | Passes | No change in color or gloss. No blistering, peeling, flaking or cracking observed. |
8) | Salt Spray Test (5% Na Cl) 100 hrs. | IS 13630 (part 8) 2006 | Passes | No change in surface. No blistering, peeling, flaking or cracking observed |
9) | Stain Test (methylene blue & potassium permanganate)) | IS 13630 (part 8) 2006 | Passes | Class I. Stain removed by water. |
10) | Modulus of Rupture, Kg/Cm2 | IS 13630 (part 6) 2006 | 100 kg/sq cm. | |
11) | Water Absorption, % | 24 hours soaking in water | 18 by weight 33 by volume |
More pores: more insulation. Or less conductivity. |
12) | Crazing Test | IS 13630 (part 9) | 4 cycle passes |
Fix hollow tile with necessary slope to drain rain water. Plaster the surface with water proof compounds. Air circulation in hollow tiles is very much advantageous.
Coat I:
Primer Coat: Mixture of grey cement and acrylic polymer with fine sand and PPF to be brushed.
Coat II:
White Coat: Titanium mixed with Roof Tiles white powder and acrylic polymer, fine sand and PPF to be brushed on Primer Coat.
Coat III:
White Coat: Titanium mixed with Roof Tiles White powder and acrylic polymer and PPF to be brushed on second coat.
Coat IV:
Final protective coat of Roof Tiles Nano White to be applied on white coat.
Specifications are subject to change for improvement without any prior information.