We are emerged as accomplish global suppliers of Raw and processed Botanical products of Indian origin. With the help of our thorough search and well integrated vendor network, we gained expertise in sourcing, processing and packaging of various botanical products from India. Our products are extensively used by Ayurvedic, Herbal, Pharmaceutical,More..
tamarind kernel powder :
we offer finest quality tamarind kernel powder for gum, textile, paper, plywood & other industrial applications.kernel is inner portion of the seeds. Tamarind kernel powder is obtain from this kernel. It is composed of glucose, xylose and galactose in a ratio 3:2:1. And has a high molecular weight ranging from 2.5x105to 6.5x105.it is better gelling agent. The solution is very stable in wide range of temperature & ph. The viscosity of tkp is directly proportional to its concentration, it increases sharply even with small increase in the concentration. Viscosity is not impacted by ph of the solution, or by iron, sodium salts. It performs better in presence of sugars.
technical details:
01] colour creamy white
02] appearance fine powder
03] odour characterastic, almost odourless
04] crude fibre 1 2 %
05] ph 6 7 %
06] tannins unknown
07] lipids -- 6- 10 %
08] proteins 18 20 %
09] insoluble 1 2 %
10] ash 1 3 %
11] moisture 6 12 %
12] viscosity 2800 -- 3200 cps 3 % solution
tkp vs pectin:
tkp in the aqueous media forms mucilaginous dispersion and exhibit characteristics of gelling in presence of sugar concentrates, analogous to the pectin. Unlike pectin, tkp can gel at various ph, (including ph levels 7 and above). Also aqueous solutions of tkp are more thermal stable as compared to those of pectin. Tkp shows a strong affinity towards most of the natural gums (especially cellulose) and would show synergism to them.
tkp vs guar gum:
tkp shows better thermal stability than guar gum. Also the ph tolerance is higher in tkp. Guar gum is far most superior than tkp in dispersion and suspension. Guar gum is readily soluble in cold water, whereas tkp takes more time for achieving full viscosity.