Our Products
We offer the best product range of Diamond Compound, CBN & Bakelite Bonded Cutting Blades, Polishing Pads, Graphene Nanoplatelets (1-2nm) and Graphite Cylindrical Crucible.
| Units of Measure | Value | |
| Density | gm/cc (lb/ft3) | 2.2 |
| Porosity | %(%) | 0 |
| Tensible Strength | 106 Pa | 48.3 |
| Young’s Modulus | 106 Pa | 71.7 |
| Hardness | kg/mm2 | 600 |
| Thermal Conductivity | W/m°K | 1.38 |
| Coefficient of Thermal Expansion | 10-6/°C | 0.55 |
| Specific Heat | J/Kg°K | 740 |
| Dieletric Strength | Ac-kv/mm (volts/mil) | 30 |
| Dieletric Constant | @1MHz | 3.82 |
| Index of refraction @ 587.6nm | — | 1.4585 |
Physical Properties of Lid for Tall Form Quartz Crucible
| Units of Measure | Value | |
| Density | gm/cc (lb/ft3) | 2.2 |
| Porosity | %(%) | 0 |
| Tensible Strength | 106 Pa | 48.3 |
| Young’s Modulus | 106 Pa | 71.7 |
| Hardness | kg/mm2 | 600 |
| Thermal Conductivity | W/m°K | 1.38 |
| Coefficient of Thermal Expansion | 10-6/°C | 0.55 |
| Specific Heat | J/Kg°K | 740 |
| Dieletric Strength | Ac-kV/mm (volts/mil) | 30 |
| Dieletric Constant | @1MHz | 3.82 |
| Index of refraction @ 587.6nm | — | 1.4585 |
| Units of Measure | Value | |
| Density | gm/cc (lb/ft3) | 2.2 |
| Porosity | %(%) | 0 |
| Tensible Strength | 106 Pa | 48.3 |
| Young’s Modulus | 106 Pa | 71.7 |
| Hardness | kg/mm2 | 600 |
| Thermal Conductivity | W/m°K | 1.38 |
| Coefficient of Thermal Expansion | 10-6/°C | 0.55 |
| Specific Heat | J/Kg°K | 740 |
| Dieletric Strength | Ac-kv/mm (volts/mil) | 30 |
| Dieletric Constant | @1MHz | 3.82 |
| Index of refraction @ 587.6nm | — | 1.4585 |
| Units of Measure | Value | |
| Density | gm/cc (lb/ft3) | 2.2 |
| Porosity | %(%) | 0 |
| Tensile Strength | 106 Pa | 48.3 |
| Young’s Modulus | 106 Pa | 71.7 |
| Hardness | kg/mm2 | 600 |
| Thermal Conductivity | W/m°K | 1.38 |
| A coefficient of Thermal Expansion | 10-6/°C | 0.55 |
| Specific Heat | J/Kg°K | 740 |
| Dielectric Strength | Ac-kV/mm (volts/mil) | 30 |
| Dielectric Constant | @1MHz | 3.82 |
| Index of refraction @ 587.6nm | — | 1.4585 |
Features :
Uses :
| Approximate Weight in gm | |||||
| Code | Capacity (ml) | Top Diameter (mm) | Height (mm) | Crucible | Lid |
| PMCru1 | 1 | 12 | 13 | 2 | 0.5 |
| PMCru3 | 3 | 17 | 19 | 4.5 | 1.5 |
| PMCru5 | 5 | 20.5 | 22 | 5.5 | 1.75 |
| Units of Measure | Value | |
| Density | gm/cc (lb/ft3) | 2.2 |
| Porosity | %(%) | 0 |
| Tensible Strength | 106 Pa | 48.3 |
| Young’s Modulus | 106 Pa | 71.7 |
| Hardness | kg/mm2 | 600 |
| Thermal Conductivity | W/m°K | 1.38 |
| Coefficient of Thermal Expansion | 10-6/°C | 0.55 |
| Specific Heat | J/Kg°K | 740 |
| Dieletric Strength | Ac-kv/mm (volts/mil) | 30 |
| Dieletric Constant | @1MHz | 3.82 |
| Index of refraction @ 587.6nm | — | 1.4585 |
| Approximate Weight in gm | ||||||
| Code | Capacity (ml) | Top Diameter (mm) | Height (mm) | Crucible | Reinforced Rim | Lid |
| PCruLF10 | 10 | 29 | 24 | 8 | 9.5 | 3 |
| PCruLF15 | 15 | 32 | 26 | 13 | 15 | 5 |
| PCruLF20 | 20 | 37 | 30 | 16 | 18 | 5 |
| PCruLF25 | 25 | 41 | 34 | 20 | 23 | 6.5 |
| PCruLF35 | 35 | 44 | 36 | 30 | 33 | 8.5 |
| PCruLF50 | 50 | 49 | 40 | 42 | 45 | 10 |
| PCruLF70 | 70 | 55 | 45 | 60 | 64 | 16 |
| Approximate Weight in gm | ||||||
| Code | Capacity (ml) | Top Diameter (mm) | Height (mm) | Crucible | Reinforced Rim | Lid |
| PCruHF10 | 10 | 26 | 29 | 8 | 9.5 | 2.5 |
| PCruHF15 | 15 | 29 | 33 | 11 | 13 | 4 |
| PCruHF20 | 20 | 32 | 36 | 16 | 18 | 4.5 |
| PCruHF25 | 25 | 35 | 39 | 20 | 23 | 5 |
| PCruHF30 | 30 | 37 | 41 | 25 | 28 | 5 |
| PCruHF35 | 35 | 39 | 43 | 29 | 32 | 6 |
| PCruHF40 | 40 | 41 | 46 | 33 | 36.5 | 7 |
| PCruHF50 | 50 | 44 | 49 | 42 | 46 | 8 |
| PCruHF75 | 75 | 50 | 55 | 60 | 65 | 10 |
| PCruHF100 | 100 | 56 | 62 | 80 | 85 | 16 |