Typical Room Temperature Tensile Properties
| Condition | 0.2% Yield Strength | Ultimate Tensile Strength | % Elongation in 4D | % Reduction of Area | ||
|---|---|---|---|---|---|---|
| ksi | MPa | ksi | MPa | |||
| Typical | 55 | 379 | 110 | 758 | 60 | 70 |
| ASTM B574 (min) | 41 | 283 | 100 | 690 | 40 | - |
Chemical Composition, %
| Nia | Co | Cr | Mo | W | Fe | Si | Mn | C | Others |
|---|---|---|---|---|---|---|---|---|---|
| 57 | 2.5** | 16 | 16 | 4 | 5 | 0.08** | 1** | 0.01** | V-0.35** |
*The undiluted deposited chemical composition of Hastelloy C276 covered electrodes has 0.02 percent maximum carbon, 0.20 percent maximum silicon, 0.03 percent maximum phosphorus, and 0.015 percent maximum sulfur. **Maximum a= As Balance