Our Products
We have manufacturing all kind of tmt bars. For a example fe500/500d/550/crs/hcrm/ms rounds/special lengh sizes as per customers request.
Additional Information:
Payment Terms : L/C, D/P, T/T,
Packaging Details : Loose/container
Delivery Time : Max 10days
Our Whole process of TMT bar manufacture is housed in a single compound ensuring a continuous process for unmatched quality. The most advanced technology from German & sophisticated machinery is employed in the manufacture of the bars. 100 % German Automatic Rolling Mill & German Thermex QST technology rollout highest quality TMT bars.
Mechanical And Chemical Properties
Rebar Grade (%) | BIS 500 | Kamachi 500 Typical Values | |
---|---|---|---|
Carbon | 0.3 | 0.25 | |
Silicon | - | 0.15-0.25 | |
Manganese | - | 0.55 | |
Sulphur (MAX ) | 0.06 | 0.05 | |
Phosphorous (MAX) | 0.06 | 0.05 | |
Sulphur + Phosphorous (MAX) | 0.11 | 0.1 | |
Carbon Equivalent (CE) | 0.42 | 0.32-0.38 | |
Copper (MIN) | - | - | |
Chromium | - | - | |
Yield Stress (N/mm2) Min | 500 | 525 | |
Elongation (MIN) | 12 | 16 | |
Ultimate Tensile Strength | 545 | 600 | |
Uts/Ys Ratio | 1.08 | 11 |
Mechanical And Chemical Properties
Rebar Grade (%) | BIS 500 D | Kamachi 500 D Typical Values |
---|---|---|
Carbon | 0.25 | 0.20-0.25 |
Silicon | - | 0.15-0.25 |
Manganese | - | 0.90-100 |
Sulphur (MAX ) | 0.04 | 0.35 |
Phosphorous (MAX) | 0.04 | 0.04 |
Sulphur + Phosphorous (MAX) | 0.075 | 0.07 |
Carbon Equivalent (CE) | 0.42 | 0.31-0.36 |
Copper (MIN) | - | - |
Chromium | - | - |
Yield Stress (N/mm2) Min | 500 | 525 |
Elongation (MIN) | 16 | 18 |
Ultimate Tensile Strength | 565 | 600 |
Uts/Ys Ratio | 1.1 | 1.15 |
Mechanical And Chemical Properties
Rebar Grade (%) | BIS FE 600 | Kamachi FE 600 Typical Values | |
---|---|---|---|
Carbon | 0.3 | 0.25 | |
Silicon | - | 0.15-0.25 | |
Manganese | - | 0.95-1.05 | |
Sulphur (MAX) | 0.04 | 0.04 | |
Phosphorous (MAX) | 0.04 | 0.04 | |
Sulphur + Phosphorous (MAX) | 0.08 | 0.08 | |
Carbon Equivalent (CE) | 0.42 | 0.42 | |
Copper (min) | - | - | |
Chromium | - | - | |
Yield Stress (N/ Mm2) Min | 600 | 630 | |
Elongation (MIN) | 10 | 11 | |
Ultimate Tensile Strength | 660 | 670 | |
Uts/Ys Ratio | 1.06 | 1.05 |
Mechanical And Chemical Properties
Rebar Grade (%) | Kamachi FE 500D HCRM Typical Values |
---|---|
Carbon | 0.35 |
Silicon | 0.35 |
Manganese | 0.80-1.00 |
Sulphur (MAX ) | 0.04 |
Phosphorous (MAX) | 0.090 |
Sulphur + Phosphorous (MAX) | 0.130 |
Carbon Equivalent (CE) | 0.53 |
Copper (MIN) | 0.20-0.30 |
Chromium | 0.40-0.50 |
Yield Stress (N/mm2) Min | 525 |
Elongation (MIN) | 18 |
Ultimate Tensile Strength | 600 |
Uts/Ys Ratio | 1.15 |