Material
Copper With Arsenic Alloy
-
Number Of Flower
Rod
-
Feature
High Tensile Strength, Ductile, Durable, Corrosion Resistant
-
Application
Boiler Fireboxes, Wood Preservatives
-
Chemical Properties
0.01 Max, 0.01 Max, 0.15 Max, 0.03 Max, 0.30 - 0.50, 0.013 - 0.05, 99.20 Min, 0.01 Max, 0.003 Max, 0.02 Max, 0.07 Max
Arsenic Copper Rod offered by us, that is manufactured using advanced technologies, which ensures high efficiency. These rods are used in various industries and known for their high ductility and durability. We are listed as one of the prominent Manufacturers and Exporters of Arsenic Copper Rod.Features :High tensile strengthDuctileDurableCorrosion resistantUsed in :Boiler FireboxesWood preservativesTechnical Specifications:- Chemical PropertiesSn0.01 Max.Pb0.01 Max.Ni0.15 Max.Fe0.03 Max.As0.30 - 0.50P0.013 - 0.05Cu + Ag99.20 MinSb0.01 Max.Bi0.003 Max.Se + Te0.02 Max.Total Impurities (Excl.Ag, Ni, As & P) 0.07 Max
| Annealed | Hard | Hard1 | Hard2 |
| %Elongation at 5.65Sq.Rt So G.L. | 35.00+Min. | 15.00+Min. | 20.00+Min. | 20.00+Min. |
| Hydrogen Embrittlement Test | Reqd. | Reqd. | Reqd. | Reqd. |
| Size | Over+10+mm+ | Over+10+mm +to+16+mm | Over+16+mm+ to+25+mm | Over+25+mm+ |
| U.T.S. h bar | 21.00+Min | 28.00+Min. | 25.00+Min. | 24.00+Min |