Property
Tensile strength ., Tensile strength after aging
-
Requirements
8 N/mm2 (min) , 7N/mm2 (min.)
-
Test Method
ASTM D 638 , ASTM D 2671/120oC , 168 hrs.
DBIT is made from radiation cross linked polyolefinThe dual layer structure of insulationhot melt adhesiveWidely used to protect complex busbar connections where tube products can not be appliedUp to 24 KV