Contact SupplierThin Layer Polymer Modified Concrete / AAC Block Joining Mortar Advantages
| Sr No | Properties | Specifications |
| 1 | Appearance | Free flowing Powder |
| 2 | Color | Grey |
| 3 | Water Requirement | 30 to 35% |
| 4 | Workability | Better than conventional mortar |
| 5 | Pot Life | 2 hrs @ 30.C |
| 6 | Compressive Strength @ 28 Days | 40 Kgs / Sq. Cm. |