    When barrel finishing plastic optical frames, the normal workload for one compartment of a 30" x 36" dry tumbling barrel is 200 heavyweight fronts or 250 lightweight fronts. Twice this amount can be....
    View More Details
    Send Enquiry

    Company Information

    • calendar Member Since 18 Years
    • building Nature of Business Supplier

    Ask for more detail from the seller

    Contact Supplier
    Report incorrect details

    Product Details no_img_icon

    When barrel finishing plastic optical frames, the normal workload for one compartment of a 30" x 36" dry tumbling barrel is 200 heavyweight fronts or 250 lightweight fronts. Twice this amount can be added at one time when tumbling temples. The ratio (by volume) of hardwood media to frames should be at least three to one. This applies to all steps listed below. If nose panels are very rough, they should be ashed on a buff before tumbling.
    Step 1
    This step will remove tool marks, round off edges and leave a satin finish. The load height should be approximately three inches below center. Start with 5 lb of coarse Dry Abrasive Cream (10 lb if using new pegs). After 16-24 hours, add 5 lb of fine Dry Abrasive Cream (10 lb if using new pegs). Before unloading, run the barrel with screen doors for approximately one hour to remove old compound and extra plastic.
    Step 2
    This step will produce a smooth surface and keep parts clean. The load height should be approximately at the center. Use 5 lb of Shynolyte Pre-Polishing Cream (10 lb if using new pegs). Run the barrel for 24 hours. Before unloading, run the barrel with screen doors for approximately one hour. Hinges can be installed after this process.
    Step 3
    This step is used to run the parts with hinges installed. This step will remove scratches created when slotting and installing hinges. The load height should be approximately at the center. Use one tablespoon of Shynolyte Pre-Polishing Cream for each run. Run the barrel for about 24 hours. (To break in new pegs, use one pint of Shynolyte Pre-Polishing Cream and run the pegs for a few hours without parts.)
    Step 4
    This step will produce a high luster. The load height should be approximately at the center. Use one tablespoon of Microlyte Polishing Cream for each run. Run the barrel for about 24 hours. (To break in new pegs, use one pint of Microlyte Polishing Cream and run the pegs for a few hours without parts.)


    Share your requirements for a quick response!
    Tell us what you need?

    Looking for Barrel Finishing Plastic Optical Frames?

    Quantity
    Seller Contact Details
    To list your productBoost Your Business Visibility WorldwideRegister Now
    To list your productBoost Your Business Visibility WorldwideRegister Now
    Waiting for permission
    To search by voice, go to your browser settings and allow access to microphone

    Allow microphone access to search with voice