Contact Supplier| Index | Standard | Oxidized Bitumen Grade | |||||
| 75/30 | 85/25 | 85/40 | 95/25 | 105/35 | 115/15 | ||
| Softening Point Temperature(°C) | ASTM D36 | 75±5 | 85±5 | 85±5 | 95±5 | 105±5 | 115±5 |
| Penetration at 25 C (dmm) | ASTM D5 | 30±5 | 25±5 | 40±5 | 25±5 | 35±5 | 15±5 |
| Thermal Loss Percentage | ASTM D1754 | 0.2 | 0.2 | 0.5 | 0.2 | 0.2 | 0.2 |
| Solubility in trichloroethylece | ASTM D2042 | 99.5 | 99.5 | 99.5 | 99.5 | 99.5 | 99.5 |
| Test | Method | 30-40 | 40-50 | 60-70 | 85-100 | 110-120 |
|---|---|---|---|---|---|---|
| Density | ASTM D-7 | 1/01-1/06 | 1/01-1/06 | 1/01-1/06 | 1/01-1/05 | 1/01-1/04 |
| Pentration Rate at 25°C, 10/mm | ASTM D-5 | 30-40 | 40-50 | 60-70 | 85-100 | 100-120 |
| Softening Point°C | ASTM D-36 | 55-63 | 52-60 | 49-56 | 45-52 | 42-49 |
| Ductility at 25°C(cm)-min | ASTM D-113 | 100 | 100 | 100 | 100 | 100 |
| Flash Point °C-min | ASTM D-92 | 250 | 250 | 250 | 250 | 250 |
| Solubility in Disulfide %wt-max | ASTM D-4 | 99.5 | 99.5 | 99.5 | 99.5 | 99.5 |
| Stain Test | AASHTO T 102 | Negative | ||||
| Weight Loss by heating %wt-max | ASTM D-6 | 0.2 | 0.2 | 0.2 | 0.2 | 0.2 |
| Penetration Loss by Heating %-max | ASTM D-6-D-5 | 20 | 20 | 20 | 20 | 20 |