Contact SupplierExtremely Low density 0.80 – 0.85 g/cc which is 50-60% of the ordinary perlite.
2) Expansion is 36cc against 23-24 cc of Ordinary perlite.
3) Addition rate is max 0.15% against 0.3-0.4% of perlite.
4) No spirting of metal results in high METAL cleanliness surrounding the furnace &
inside the plant.
5) Highest quality of Slag Coagulation & will help in minimizing rejection due to slag
inclusion at foundry as well as after machining stage.