- Supply TypeManufacturer, Exporter, Supplier
- Preferred Buyer Location All over the world
1) using vacuum pressure and dipping in the sodium silicate liquid. 2) heating and adding the acid to make the silicon dioxide. 3) keeping the pressure be 0.6mp under the vacuum situation. 4) reduce the porosity by more than 70% after dippting in the sodium silicate liquid.