Contact Supplier| Property | Units | Test Method | Value | ||
| Thickness | Micron | ISO 4593 | 12 | 15 | 25 |
| Yield | m2/kg | ASTM D1505 | 71.58 | 58.4 | 34.53 |
| Barrier | |||||
| OTR @ 77 °F (25°C) /0% RH | cc/m2/day | ASTM D3985 | 36 | 33 | 25 |
| WVTR @ 100 °F (37.8°C) /100% RH | g/m2/day | ASTM F1249 | 85 | 70 | 50 |
| Optical | |||||
| Gloss (at 45 degree) | % | ASTM D 2457 | 105 | 105 | 100 |
| Haze | % | ASTM D 1003 | 2.7 | 2.7 | 3.2 |
| Physical | |||||
| Tensile strenth at break (MD/TD) | Mpa | ASTM D882 | 250/290 | 250/290 | 250/290 |
| Elongation (MD/TD) | % | ASTM D882 | 145/100 | 145/100 | 150/100 |
| Modulus (Elastic)Â Â (MD/TD) | Mpa | ASTM D882 | 2500/1500 | 2500/1500 | 2500/1500 |
| Thermal | |||||
| Shrinkage  MD | % | ASTM D1204 | 1.0-1.5 | 1.0-1.5 | 1.0-1.5 |
| Shrinkage  TD | % | ASTM D1204 | 0.8-1.5 | 0.8-1.5 | 0.8-1.5 |
| Coefficient of Friction | |||||
| Untreated | Â | ASTM D1894 | 0.29 | 0.29 | 0.29 |
| Treated | Â | ASTM D1894 | 0.29 | 0.29 | 0.29 |
| Surface Tension | |||||
| Untreated | mN/m | ASTM D2578 | 53 | 53 | 53 |
| Treated | mN/m | ASTM D2578 | 53 | 53 | 53 |