Contact Supplier| Test Method | Properties | Unit | Specification |
| Lab Test | Color | Visually | Black |
| ASTM D 3652 | Total Thickness | Micron | 130±10 |
| ASTM D 3330 | Peel strength | N/25mm | ≥2 |
| ASTM D 3759 | Tensile Strength | N/25mm | ≥20 |
| ASTM D 3121 | Rolling ball tack | mm | ≤100 |
| ASTM D 3654 | Holding power | Hour | NA |
| Lab test | Temperature resistance ( 30 minutes) | ºC | 70ºC max |
| Lab test | Application temperature | ºC | 10 ºC to 55ºC |