Company Information
Ask for more detail from the seller
Contact SupplierReclaimed Rubber produced from the process of de-vulcanisation (recycling) of rubber scrap & waste rubber. In the tire reclaimed rubber process de-vulcanization begins with the delinking of the sulfur elements from the rubber elements, therefore reclaiming agent, processing oil and pine tar are added in crumbed rubber powder at high temperature & pressure, thereby enabling the adjectives of either natural or synthetic rubber to be reproduced.
| Chemical Properties | Superfine- HR Reclaim Rubber | Fine- 111 Reclaim Rubber | Medium -202 Reclaim Rubber | Coarse- 303 Reclaim Rubber | |||||
|---|---|---|---|---|---|---|---|---|---|
| Ash % | 8 ± 2 | 8 ± 2 | 8± 2 | 8 ± 2 | |||||
| Carbon Black % | 27 ± 3 | 27 ± 3 | 27 ± 3 | 27 ± 3 | |||||
| Acetone Extract % | 15 ± 3 | 15 ± 3 | 15 ± 3 | 15 ± 4 | |||||
| RHC Difference % | 47 min. | 47 min | 47 min | 47 min | |||||
| Physical Properties | |||||||||
| Specific Gravity % | 1140 ± 20 | 1140 ± 20 | 1140 ± 20 | 1140 ± 20 | |||||
| Tensile Strength Kg/cm2 | 55 min | 40 min | 35 min | 25 min | |||||
| Elongation at Break % | 240 min | 220 min | 200 min | 180 min | |||||
| Hardness Shore A | 59±3 | 59±3 | 59±3 | 59±3 | |||||
| Mooney Viscisity | 25-45 | 25-45 | 25-45 | 25-55 | |||||
| Physical Appearance | Black Sheet 50 KG Packing in Export Worthy Low Weight Bags | ||||||||
| Application | Superfine-HR Max PHP | Fine-111 Max PHP | Medium-202 Max PHP | Coarse-303 Max PHP | |||||
| Auto Tyres | 10 | 10 | 10 | 10 | |||||
| Cycle Tyres | 40 | 40 | 40 | 40 | |||||
| Tread Rubber | 20 | 20 | 20 | 20 | |||||
| Molded Goods | 40 | 40 | 40 | 40 | |||||
| Footwears | 30 | 30 | 30 | 30 | |||||
| Mattings | 60 | 60 | 60 | 60 | |||||
| Conveyor Belts | 30 | 30 | 30 | 30 | |||||
| Battery Containers | 80 | 80 | 80 | 80 | |||||