Our product range contains a wide range of Whole Tyre Reclaim Rubber

Whole Tyre Reclaim Rubber

  • Ash % 8 ± 2
  • Carbon Black % 27 ± 3
  • Acetone Extract % 15 ± 3
  • Specific Gravity % 1140 ± 20
  • Tensile Strength Kg/cm2 25 - 55 min
  • Mooney Viscisity 25-45

Reclaimed Rubber produced from the process of de-vulcanisation (recycling) of rubber scrap & waste rubber. In the tire reclaimed rubber process de-vulcanization begins with the delinking of the sulfur elements from the rubber elements, therefore reclaiming agent, processing oil and pine tar are added in crumbed rubber powder at high temperature & pressure, thereby enabling the adjectives of either natural or synthetic rubber to be reproduced.

Technical Specification Of Reclaimed Rubber

Chemical Properties Superfine- HR
Reclaim Rubber
Fine- 111
Reclaim Rubber
Medium -202
Reclaim Rubber
Coarse- 303
Reclaim Rubber
Ash % 8 ± 2 8 ± 2 8± 2 8 ± 2
Carbon Black % 27 ± 3 27 ± 3 27 ± 3 27 ± 3
Acetone Extract % 15 ± 3 15 ± 3 15 ± 3 15 ± 4
RHC  Difference % 47 min. 47 min 47 min 47 min
Physical Properties
Specific Gravity % 1140 ± 20 1140 ± 20 1140 ± 20 1140 ± 20
Tensile Strength Kg/cm2 55 min 40 min 35 min 25 min
Elongation at Break % 240 min 220 min 200 min 180 min
Hardness Shore A 59±3 59±3 59±3 59±3
Mooney Viscisity 25-45 25-45 25-45 25-55
Physical Appearance Black Sheet
50  KG Packing in Export Worthy Low Weight Bags
Application Superfine-HR
Max PHP
Fine-111
Max PHP
Medium-202
Max PHP
Coarse-303
Max PHP
Auto Tyres 10 10 10 10
Cycle Tyres 40 40 40 40
Tread Rubber 20 20 20 20
Molded Goods 40 40 40 40
Footwears 30 30 30 30
Mattings 60 60 60 60
Conveyor Belts 30 30 30 30
Battery Containers 80 80 80 80