Our Products
Our offered Product range includes Alloy 20 Round Bar, Waspaloy Round Bar, Super Duplex Round Bar, L605 Round Bar and Haynes Round Bar.
| STANDARD | WERKSTOFF NR. | UNS |
| Inconel X750 | 2.4669 | N07750 |
| Grade | Ni | Cr | Al | C | Mn | Ti | Cu | Si | S |
| Inconel X-750 | 70.0 min | 14.0 - 17.0 | 0.40 - 1.0 | .08 max | 1.00 max | 2.25 - 2.75 | 0.50 max | .50 max | .01 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.28 g/cm3 | 1430°C | 1267 MPa | 868 MPa | 25 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| SS 422 | 1.4742 | S42200 | SUS 422 | 442S19 | – | – | – |
| Grade | C | Si | Ni | S | Mn | P | Cr | Mo | V | Cu | W | |
| SS 422 | min. | 0.20 | 0.20 | 0.50 | - | - | - | 11.0 | 0.75 | 0.17 | - | 0.90 |
| max. | 0.25 | 0.60 | 1.00 | 0.030 | 1.00 | 0.040 | 13.5 | 1.25 | 0.30 | 0.50 | 1.25 | |
| Grade | Tensile Strength (MPa) min | Elongation (% in 50mm) min | Yield Strength 0.2% Proof (MPa) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| Stainless Steel 422 | 115 | 25 | 140 | 293 | 341 |
| STANDARD | WERKSTOFF NR. | UNS |
| Hastelloy X | 2.4665 | N06002 |
| Grade | Ni | Mo | Cr | Fe | Mn | C | Co | Si | P | S |
| Hastelloy X | Balance | 8.00 - 10.00 | 20.50 - 23.00 | 17.00 - 20.00 | 1.00 max | 0.05 - 0.15 | 0.50 - 2.50 | 1.00 max | 0.04 max | 0.03 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.22 g/cm³ | 1355°C | 655 MPa | 240 MPa | 35% |
| STANDARD | WERKSTOFF NR. | UNS |
| Nimonic 90 | 2.4632 | N07090 |
| Grade | C | Cr | Co | Ti | Al | Si | Cu | Mn |
| Nimonic Alloy 90 | 0.2 max | 18 - 21 | 15 - 21 | 2 - 3 | 1 - 2 | 1.0 max | 0.2 max | 1.0 max |
| Density | Melting Point | Coefficient of Expansion | Modulus of Rigidity | Modulus of Elasticity (Annealed + Aged) (Spring Temper + Aged) |
| 8.18g/cm³ | 1370°C | 12.7 μm/m °C (20 - 100°C) | 82.5 kN/mm² | 213 kN/mm² 227 / 240 kN/mm² |
| STANDARD | WERKSTOFF NR. | UNS | JIS | GOST | EN | OR |
| Hastelloy C276 | 2.4819 | N10276 | NW 0276 | ХН65МВУ | NiMo16Cr15W | ЭП760 |
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| C276 | 0.010 max | 1.00 max | 0.08 max | 0.03 max | 2.50 max | 50.99 min* | 14.50 – 16.50 | 4.00 – 7.00 | 15.00 – 17.00 | 0.04 max |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Hastelloy C276 | 8.89 g/cm3 | 1370 °C (2500 °F) | Psi – 1,15,000 , MPa – 790 | Psi – 52,000 , MPa – 355 | 40 % |
| STANDARD | UNS | WERKSTOFF NR. |
|---|---|---|
| ASTM A105 | K03504 | – |
| Carbon Steel | C | Si | Mn | P | S | Cr |
|---|---|---|---|---|---|---|
| A105 | 0.35 | 0.10-0.35 | 0.60-1.05 | 0.035 | 0.040 | 0.30 |
| Tensile Strength (N/mm2) | Elongation % | HB max |
|---|---|---|
| 485 | 22 | 187 |
| STANDARD | WERKSTOFF NR. | UNS | GOST | AFNOR | JIS | BS | EN |
| Monel 400 | 2.4360 | N04400 | МНЖМц 28-2,5-1,5 | NU-30M | NW 4400 | NA 13 | NiCu30Fe |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | W |
| Monel 400 | 0.010 max | 0.50 max | 0.08 max | 0.02 max | 0.02 max | 20 - 22.5 | 12.5 - 14.5 | Bal | 2.5 - 3.5 |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.69 g/cm3 | 1399 °C (2550 °F) | Psi – 1,00,000, MPa–690 | Psi – 45000, MPa–310 | 45 % |
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| Inconel X750 | 0.08 max | 1.00 max | 0.5 max | 0.01 max | 0.5 max | 9.0 max | 70.0 min | 17 max |
| STANDARD | WERKSTOFF NR. | UNS |
| Inconel X750 | 2.4669 | N07750 |
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Inconel X-750 | 0.08 max | 1.00 max | 0.5 max | 0.01 max | 0.5 max | 5.0-9.0 | 70 max. |
| STANDARD | WERKSTOFF NR. | UNS |
| Inconel X-750 | 2.4669 | N07750 |
| Grade | Ni | Cr | Co | Ti | Al | C | Si | Cu | Fe | Mn | B | S | Zr | Pb |
| Nimonic 90 | Bal | 18-21 | 15-21 | 2-3 | 1-2 | 0.2 max | 1.0 max | 0.2 max | 1.5 max | 1.0 max | 0.02 max | 0.015 max | 0.15 max | 0.0020 max |
| Grade | Material Sheet |
Temperature °C | Yield Strength 0.2 % (MPa) | Tensile Strength (MPa) | Elongation (%) | Hardness HV |
| Nimonic 90 | Nimonic 90 sheet Solution Treated (BS HR202) |
RT | – | – | – | 250 max |
| Nimonic 90 sheet Precipitation Treated (BS HR 202) |
RT | 695 min | 1080 min | 25 min (0.45mm-3.0mm) |
280 min | |
| Nimonic 90 sheet Precipitation Treated (BS HR202) |
500 | 740 (typical) | 995 (typical) | 30 | – | |
| Alloy 90 Cold Rolled Sheet (Heat Treated) |
– | – | – | – | – |
| STANDARD | WERKSTOFF NR. | UNS |
| Nimonic 90 | 2.4632 | N07090 |
| STANDARD | WERKSTOFF NR. | UNS |
| Monel R405 | – | N04405 |
| Grade | Fe | C | Ni | Mn | Si | S | Cu | Al |
| Monel R405 | 2.5 max | 0.3 max | 63 min | 2.0 max | 0.5 max | 0.025 – 0.060 | 28.0-34.0 | – |
| STANDARD | WERKSTOFF NR. | UNS |
| Monel K500 | 2.4375 | N05500 |
| Grade | Ni | Fe | C | Mn | Si | Cu | Al | S | Ti |
| Monel K500 | 63.0 min | 0.5 – 2 | 0.25 max | 1.5 max | 0.5 max | 27.0 – 33.0 | 2.3 – 3.15 | 0.010 max | 0.35 – 0.85 |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.44 g/cm3 | 1350 °C (2460 °F) | Psi – 160000 , MPa – 1100 | Psi – 115000 , MPa – 790 | 20 % |
| STANDARD | WERKSTOFF NR. | UNS |
|---|---|---|
| Nimonic Alloy 75 | – | N06075 |
| Grade | C | Ni | Cu | Cr | Ti | Fe | Mn |
|---|---|---|---|---|---|---|---|
| Nimonic Alloy 75 | 0.08 / 0.15 | Bal | 0.5 max | 18.9 – 21.0 | 0.2 / 0.6 | 5.0 max | 1.0 max |
| Mechanical & Physical Properties | 21.1°C | 100°C | 204.4°C | 315.6°C | 400 °C | 537.8°C | 648.9°C | 700°C | 760 °C | 815 °C | 870 °C | 982 °C |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Ultimate Tensile Strength /MPa | 792 | – | – | – | – | 726 | 473 | – | 286 | – | 139 | 66 |
| 0.2% Yield Strength /MPa | 407 | – | – | – | – | 363 | 275 | – | 152 | – | 68 | 31 |
| Elongation % | 31 | – | – | – | – | 27 | 32 | – | 75 | – | 90 | 91 |
| 1,000 hr Rupture Strength | – | – | – | – | – | – | 83 | 47 | 26 | 15 | 8.3 | – |
| Coefficient of Thermal Expansion /µm/m°C ** | – | 11 | 12.7 | 13.4 | 13.9 | 14.3 | 15 | 15.4 | – | 16.5 | 17.1 | 18.2 |
| Thermal Conductivity /kcal/(hr.m.°C) ** | 10.06 | – | – | – | – | – | – | – | – | – | – | – |
| Modulus of Elasticity / GPa | 221 | 216 | 210 | 203 | 197 | 190 | 181 | 173 | – | 165 | 153 | 140 |
| STANDARD | WERKSTOFF NR. | UNS |
|---|---|---|
| Nimonic Alloy 80A | 2.4631 | N07080 |
| Grade | C | Ni | Cu | Cr | Ti | Fe | Mn |
|---|---|---|---|---|---|---|---|
| Nimonic Alloy 80A | 0.10 max | Bal | 0.2 max | 18.0-21.0 | 1.8-2.7 | 3.0 max | 1.0 max |
| Ultimate Tensile Strength (N/mm²) | Proof Stress (N/mm²) | Elongation (%) | Hardness (HB) |
|---|---|---|---|
| 1000 | 620 | 20 | – |
| STANDARD | WERKSTOFF NR. | UNS |
|---|---|---|
| Nimonic Alloy 263 | 2.4650 | N07263 |
| Grade | C | Cr | Co | Ti | Al | Si | Cu | Mn |
|---|---|---|---|---|---|---|---|---|
| Nimonic Alloy 263 | 0.04-0.08 | 19 – 21 | 19 – 21 | 1.90 – 2.40 | 0.60 max | 0.40 max | 0.20 max | 0.60 max |
| Mechanical properties | Test Method | As Built | Heat Treated |
|---|---|---|---|
| Tensile strength | ISO 6892-1:2009(B) Annex D | 900 ± 40 MPa | 1100 ± 30 MPa |
| Yield strength (Rp 0.2 %) | ISO 6892-1:2009(B) Annex D | 650 ± 40 MPa | 800 ± 30 MPa |
| Elongation at break | ISO 6892-1:2009(B) Annex D | 40 ± 5 % | 35 ± 5 % |
| Young’s Modulus | – | 220 ± 15 MPa | 220 ± 15 MPa |
Nickel Alloy 200/201 Bars Equivalent Grades
| STANDARD | UNS | WNR. | JIS | EN |
|---|---|---|---|---|
| Nickel 200 | N02200 | 2.4066 | NW 2200 | Ni 99.2 |
| Nickel 201 | N02201 | 2.4068 | NW 2201 | LC-Ni 99 |
Nickel Alloy 200/201 Round Bar Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
|---|---|---|---|---|---|---|---|
| Nickel 200 | 0.15 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
| Nickel 201 | 0.02 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
Nickel Alloy 200/201 Round Bars Mechanical Properties
| Grade | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|---|
| Nickel 200 | 8.9 g/cm3 | 1446 °C (2635 °F) | Psi – 67000 , MPa – 462 | Psi – 21500 , MPa – 148 | 45 % |
| Nickel 201 | 8.9 g/cm3 | 1446 °C (2635 °F) | Psi – 67000 , MPa – 462 | Psi – 21500 , MPa – 148 | 45 % |
| Standard | AISI / SAE 4130 |
| UNS | - |
| WERKSTOFF NR. | 25CrMo4, GS-25CrMo4 |
| BS 970 | 708A30, CDS110 |
| UNI | 25CrMo4 (KB), 30CrMo4 |
| JIS | SCM 420, SCM 430, SCCrM1 |
| EN name | - |
| EN # | 1.7218 |
| Grade | C | Si | Mn | Cr | Mo | P | S |
| AISI 4130 | 0.28-0.33 | 0.15-0.35 | 0.4-0.8 | 0.8-1.1 | 0.15-0.25 | 0.035 | 0.04 |
| Grade | Delivery State | T.S. N/mm2 Min |
Y.S. N/mm2 Min |
A,% Min |
Z,% Min |
Hardness, (annealing or tempering) HB,max |
Forging ratio | Grain Size (level) |
Nonmetal ratio |
| AISI 4130 | Hot rolled, forged, or heat treatment | 930 | 735 | 12 | 50 | 229 | ≥ 4:1 | ≥ 6 | ≤ 2.0 |
| Standard | AISI / SAE 4340 |
| UNS | - |
| WERKSTOFF NR. | 34CrNiMo6, 40NiCrMo8-4 |
| BS 970 | 817M40, En24 |
| UNI | 35NiCrMo6 (KB), 40NiCrMo7 (KB) |
| JIS | SNCM 447, SNB24-1-5 |
| EN name | 34CrNiMo6 |
| EN # | 1.6582, 1.6562 |
| C | Mn | Si | S | P | Cr | Ni | Mo | |
| SAE - 4340 | .38- .43 | .60 - .80 | .15 - .35 | .035 MAX | .040 MAX | .70 - .90 | 1.65 -2.00 | .20 - .30 |
| Tensile strength kgf/mm² | Yield strength kgf/mm² | Elongation % | Cross section reduction rate % | Impact value | Hardness Hb |
|---|---|---|---|---|---|
| ≧100 | ≧90 | ≧16 | ≧45 | ≧7 | 293~352 |
| STANDARD | UNS | WERKSTOFF NR. |
| ASTM A350 LF2 | K03011 | 1.0508 |
| Grade | C | Ni | Si | S | Mn | P | |
| ASTM A350 LF2 | min. | - | - | 0.17 | - | 0.6 | - |
| max. | 0.30 | 0.40 | 0.37 | 0.040 | 1.35 | 0.035 | |
| Grade | Tensile Strength (ksi) min | Elongation (% in 50mm) min | Yield Strength 0.2% Proof (ksi) min | Hardness |
| ASTM A350 LF2 | 485 | 22 | 250 | 197 |
| STANDARD | WERKSTOFF NR. | UNS |
| Duplex S31803 | 1.4462 | S31803 |
| Grade | UNS No | C % | Cr % | Ni % | P % | Si % | S % | Mo % | N % | Mn % |
| 31803 | S31803 | < 0.03 | 21.0-23.0 | 4.5-6.5 | 1.03 max | 1 max | 0.02 max | 2.5-3.5 | 0.08-0.2 | < 2.0 |
| Grade | YS (MPa) | UTS (MPa) | % Elongation | Hardness(BHN) |
| 31803 | 450 min. | 620 min. | 25 min. | 293 max. |
| C | P | Mo | Mn | S | Cr | Si | Ni | |
| EN - 24 | .35 - .45 | .040 | .20 - .40 | .45 - .70 | .040 | .90 - 1.40 | .10 - .35 | 1.30 - 1.80 |
| Max Stress | 850-1000 n/mm2 | |
| Yield Stress | 680 n/mm2 Min | Up to 150mm LRS |
| 654 n/mm2 Min | 150 to 250mm LRS | |
| 0.2% Proof Stress | 665 n/mm2 Min | Up to 150mm LRS |
| 635 n/mm2 Min | 150 to 250mm LRS | |
| Elongation | 13% Min | (9% if cold drawn) |
| STANDARD | WERKSTOFF NR. | UNS |
| Hastelloy B2 | 2.4617 | N10665 |
| Grade | Ni | Mo | Cr | Fe | Mn | C | P | S | Si |
| Hastelloy B2 | Bal | 26 - 30 | 1.0 | - | 0.1 | 0.02 | 0.04 | 0.03 | 0.1 |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 9.2 g/cm3 | 1370 °C (2550 °F) | Psi – 1,15,000 , MPa –760 | Psi – 52,000 , MPa – 350 | 40% |
| STANDARD | WERKSTOFF NR. | UNS |
| 2205 Duplex | 1.4462 | S32205 |
| Grade | UNS No | C % | Cr % | Ni % | P % | Si % | S % | Mo % | N % | Mn % |
| 2205 | S32205 | < 0.03 | 22.0-23.0 | 4.5-6.5 | 0.03 max | 1 max | 0.02 max | 3.0-3.5 | 0.14-0.20 | < 2.0 |
| Grade | YS (MPa) | UTS (MPa) | % Elongation | Hardness(BHN) |
| 2205 | 450 min. | 655 min. | 25 min. | 293 max. |
| STANDARD | WERKSTOFF NR. | UNS |
| Hastelloy B3 | 2.4600 | N10675 |
| Grade | Ni | Mo | Cr | Fe | W | Mn | C | Al | Ti | Si |
| Hastelloy B3 | 65.0 min | 28.5 | 1.5 | 1.5 | 3.0 max | 3.0 max | 0.01 max | 0.50 max | 0.2 max | 10 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 9.2 g/cm3 | 1370 °C (2550 °F) | Psi – 1,15,000 , MPa –760 | Psi – 52,000 , MPa – 350 | 40% |
| STANDARD | UNS | DIN |
| CS EN-9 Round Bar | - | - |
| Grade | C | Cr | Ni | Si | S | Mn | P | Mo |
| EN - 9 | .50 - .60 | - | - | .05 - .35 | .040 MAX | .50 - .80 | .040 MAX | - |
| Heat Treatment | Condition Tons/SQ.inch | Tensile Stress RE MPA | RP0.2 MPA | A min on 5.65so | Impac | Hardness HB | Limited Ruling Section mm | |
| IZODFT.L.b | KCV Joules | |||||||
| Normalise | 45 | 700 | - | 12 | - | - | 201-255 | 63 |
| 39 | 600 | - | 13 | - | - | 170/223 | 250 | |
| R | 45/55 | 700/850 | 385 | 14 | - | - | 201/277 | 100 |
| S | 50/60 | 775/925 | 450 | 14 | - | - | 223/277 | 63 |
| T | 55/65 | 850/1000 | 555 | 12 | - | - | 248/302 | 19 |
| STANDARD | WERKSTOFF NR. | UNS |
| Hastelloy C4 | 2.4610 | N06455 |
| Grade | Ni | Mo | Cr | Fe | Co | Mn | C | Al | Ti | Si |
| Hastelloy C4 | 65.0 min | 14 - 17 | 14 - 18 | 3.0 max | 2.0 max | 1.0 max | 0.01 max | - | 0.7 max | 0.08 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.64 g/cm3 | 1350-1400 °C | 783 | 365 | 55% |
| STANDARD | WERKSTOFF NR. | UNS | GOST | AFNOR | JIS | OR | EN |
| Hastelloy C22 | 2.4602 | N06022 | - | - | NW 6022 | - | NiCr21Mo14W |
| Grade | Ni | C | Cr | Co | Fe | Mn | Mo | P | Si | S | W | V |
| Hastelloy C22 | Bal | 0.010 max | 20 – 22.5 | 2.5 max | 2 – 6 | 0.50 max | 12.5 – 14.5 | 0.02 max | 0.08 max | 0.02 max | 2.5 – 3.5 | 0.35 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.69 g/cm3 | 1399 °C (2550 °F) | Psi – 1,00,000 , MPa – 690 | Psi – 45000 , MPa – 310 | 45 % |
| STANDARD | WERKSTOFF NR. | UNS |
| Hastelloy C2000 | 2.4675 | N06200 |
| Grade | C | Ni | Si | Fe | W | Cr | Co | Mo | Mn | V | P |
| Hastelloy C2000 | .01 | Remainder | .08 | 4.0-7.0 | 3.0-4.5 | 14.5-16.5 | 2.5 | 15.0-17.0 | 1.0 | .35 | .04 |
| Grade | Yield Strength | Tensile Strength | Elongation at break |
| Hastelloy C2000 | 310 MPa | 690 MPa | 45% |
| STANDARD | WERKSTOFF NR. | UNS |
| Incoloy 925 | - | N09925 |
| Grade | Ni | Cr | Fe | Si | Mo | Cu | Mn | C | S | Al |
| Incoloy 925 | 42 - 46 | 19.55 - 22.5 | 22 min | 0.5 max | 2.5 - 3.5 | 1.5 - 3.0 | 1.0 max | 0.03 max | 0.03 max | 0.1 - 0.5 |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.14 g/cm3 | 1343°C | 650 | 300 | 30 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | EN |
| Inconel 600 | 2.4816 | N06600 | NCF 600 | NiCr15Fe |
| Grade | C | Mn | Si | Fe | S | Cr | Cu | Ni + Co |
| Inconel 600 | 0.15 max | 1.00 max | 0.50 max | 6.0 - 10.0 | 0.015 max | 14.0 - 17.0 | 0.50 max | 72.0 min |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.47 g/cm3 | 1413 °C (2580 °F) | Psi - 95,000, MPa - 655 | Psi - 45,000, MPa - 310 | 40 % |
| STANDARD | UNS | BS | EN | WERKSTOFF NR. | GOST | JIS | OR | AFNOR |
| Inconel 601 | N06601 | NA 49 | NiCr23Fe | 2.4851 | XH60BT | NCF 601 | ЭИ868 | NC23FeA |
| Grade | Ni | Cr | Fe | C | Mn | S | Si | Cu |
| Inconel 601 | 58.0 - 63.0 | 21.0 -25.0 | Balance | 0.10 max | 1.0 max | 0.015 max | 0.5 max | 1.0 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.1 g/cm3 | 1411 °C (2571 °F) | Psi – 80,000 , MPa – 550 | Psi – 30,000 , MPa – 205 | 30 % |
| STANDARD | UNS | WERKSTOFF NR. | AFNOR | EN | JIS | BS | GOST | OR |
| Inconel 625 | N06625 | 2.4856 | NC22DNB4M | NiCr22Mo9Nb | NCF 625 | NA 21 | ХН75МБТЮ | ЭИ602 |
| GRADE | Ni | C | Fe | Si | Mn | S | Al | Ti | Nb + Ta | P | Mo | Cr2 |
| Inconel 625 | 58.0 min | 0.10 max | 5.0 max | 0.50 max | 0.50 max | 0.015 max | 0.40 max | 0.40 max | 3.15–4.15 | 0.015 max | 8.0-10.0 | 20.0-23.0 |
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 8.4 g/cm3 | 1350 °C (2460 °F) | Psi - 75,000 , MPa - 517 | Psi - 1,35,000 , MPa -930 | 42.5 % |
| STANDARD | UNS | WNR. |
| Inconel 718 | N07718 | 2.4668 |
| C | Mn | P | S | Si | Cr | Ni | Mo | Cb | Ta | Ti | Al | Co | B | Cu |
| 0.08 | 0.35 | 0.015 | 0.015 | 0.35 | 17-21 | 50-55 | 2.8-3.30 | 4.75-5.50 | 0.05 | 0.65-1.15 | 0.20-0.80 | 1.00 | 0.006 | 0.30 |
| Ultimate Tensile Strength, psi | .2% Yield Strength psi | Elongation % | Hardness Rockwell B |
| 135,000 | 70,000 | 45 | 100 |
| STANDARD | WERKSTOFF NR. | UNS |
| Inconel 901 | 2.4662 | N09901 |
| Element | Content (%) |
| Nickel, Ni | 41-43 .5 |
| Chromium, Cr | 11-14 |
| Titanium, Ti | 2.2-2.75 |
| Silicon, Si | 1 max |
| Manganese, Mn | 0.8 max |
| Copper, Cu | 0.5 max |
| Aluminum, Al | 0.35 max |
| Carbon, C | 0.1 max |
| Phosphorus, P | 0.04 max |
| Sulfur, S | 0.04 max |
| Boron, B | 0.01 – 0.02 |
| Iron, Fe | Remainder |
Stainless Steel 304/304L/304H Round Bar/Rods Equivalent Grades
| STANDARD | UNS | WNR. | AFNOR | EN | JIS | BS | GOST |
|---|---|---|---|---|---|---|---|
| SS 304 | S30400 | 1.4301 | Z7CN18‐09 | X5CrNi18-10 | SUS 304 | 304S31 | 08Х18Н10 |
| SS 304L | S30403 | 1.4306/1.4307 | Z3CN18‐10 | X2CrNi18-9 / X2CrNi19-11 | SUS 304L | 304S11 | 03Х18Н11 |
| SS 304H | S30409 | 1.4301 | - | - | - | - | - |
Stainless Steel 304/304L/304H Round Bar Chemical Composition
| C | Mn | Si | P | S | Cr | Ni | N | |
|---|---|---|---|---|---|---|---|---|
| 304 | 0.07max | 2.0max | 0.75max | 0.045max | 0.03max | min: 18.0 max: 20.0 | min: 8.0 max: 10.5 | — |
| 304L | 0.03max | 2.0max | 0.75max | 0.045max | 0.03max | min: 18.0 max: 20.0 | min: 8.0 max: 12.0 | 0.10 max |
| 304H | min: 18.0 max:20.0 |
min: 8.0 max: 10.5 |
min: 0.04 max:0.10 |
0.75 max |
2.0 max |
0.045 max |
0.03 max |
0.10 max |
Stainless Steel 304/304L/304H Bar Mechanical Properties
| Grade | Tensile Strength ksi (min) | Yield Strength 0.2% ksi (min) | Elongation % | Hardness (Brinell) MAX | Hardness (Rockwell B) MAX |
|---|---|---|---|---|---|
| 304 | 75 | 30 | 40 | 201 | 92 |
| 304L | 70 | 25 | 40 | 201 | 92 |
| 304H | 75 | 30 | 40 | 201 | 92 |
| STANDARD | UNS | WNR. | AFNOR | EN | JIS | BS | GOST |
|---|---|---|---|---|---|---|---|
| SS 304 | S30400 | 1.4301 | Z7CN18‐09 | X5CrNi18-10 | SUS 304 | 304S31 | 08Х18Н10 |
| SS 304L | S30403 | 1.4306/1.4307 | Z3CN18‐10 | X2CrNi18-9 / X2CrNi19-11 | SUS 304L | 304S11 | 03Х18Н11 |
| SS 304H | S30409 | 1.4301 | - | - | - | - | - |
| C | Mn | Si | P | S | Cr | Ni | N | |
|---|---|---|---|---|---|---|---|---|
| 304 | 0.07max | 2.0max | 0.75max | 0.045max | 0.03max | min: 18.0 max: 20.0 | min: 8.0 max: 10.5 | — |
| 304L | 0.03max | 2.0max | 0.75max | 0.045max | 0.03max | min: 18.0 max: 20.0 | min: 8.0 max: 12.0 | 0.10 max |
| 304H | min: 18.0 max:20.0 |
min: 8.0 max: 10.5 |
min: 0.04 max:0.10 |
0.75 max |
2.0 max |
0.045 max |
0.03 max |
0.10 max |
| Grade | Tensile Strength ksi (min) | Yield Strength 0.2% ksi (min) | Elongation % | Hardness (Brinell) MAX | Hardness (Rockwell B) MAX |
|---|---|---|---|---|---|
| 304 | 75 | 30 | 40 | 201 | 92 |
| 304L | 70 | 25 | 40 | 201 | 92 |
| 304H | 75 | 30 | 40 | 201 | 92 |
| STANDARD | UNS | WNR. | AFNOR | EN | JIS | BS | GOST |
|---|---|---|---|---|---|---|---|
| SS 304 | S30400 | 1.4301 | Z7CN18‐09 | X5CrNi18-10 | SUS 304 | 304S31 | 08Х18Н10 |
| SS 304L | S30403 | 1.4306/1.4307 | Z3CN18‐10 | X2CrNi18-9 / X2CrNi19-11 | SUS 304L | 304S11 | 03Х18Н11 |
| SS 304H | S30409 | 1.4301 | - | - | - | - | - |
| C | Mn | Si | P | S | Cr | Ni | N | |
|---|---|---|---|---|---|---|---|---|
| 304 | 0.07max | 2.0max | 0.75max | 0.045max | 0.03max | min: 18.0 max: 20.0 | min: 8.0 max: 10.5 | — |
| 304L | 0.03max | 2.0max | 0.75max | 0.045max | 0.03max | min: 18.0 max: 20.0 | min: 8.0 max: 12.0 | 0.10 max |
| 304H | min: 18.0 max:20.0 |
min: 8.0 max: 10.5 |
min: 0.04 max:0.10 |
0.75 max |
2.0 max |
0.045 max |
0.03 max |
0.10 max |
| Grade | Tensile Strength ksi (min) | Yield Strength 0.2% ksi (min) | Elongation % | Hardness (Brinell) MAX | Hardness (Rockwell B) MAX |
|---|---|---|---|---|---|
| 304 | 75 | 30 | 40 | 201 | 92 |
| 304L | 70 | 25 | 40 | 201 | 92 |
| 304H | 75 | 30 | 40 | 201 | 92 |
| Standard | Werkstoff Nr. | UNS |
|---|---|---|
| SS 309 | 1.4828 | S30900 |
| C | Mn | Si | P | S | Cr | Ni | Fe | |
|---|---|---|---|---|---|---|---|---|
| 309 | 0.2 max | 2.0 max | 1.0 max | 0.045max | 0.03max | 22 24 | 12-15 | Balance |
| Grade | Tensile Strength ksi (min) | Yield Strength 0.2% ksi (min) | Elongation % | Hardness (Brinell) MAX |
|---|---|---|---|---|
| 309 | 40 | 30 | 40 | 217 |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
|---|---|---|---|---|---|---|---|
| SS 310 | 1.4841 | S31000 | SUS 310 | 310S24 | 20Ch25N20S2 | – | X15CrNi25-20 |
| SS 310S | 1.4845 | S31008 | SUS 310S | 310S16 | 20Ch23N18 | – | X8CrNi25-21 |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Fe |
|---|---|---|---|---|---|---|---|---|---|
| SS 310 | 0.015 max | 2 max | 0.15 max | 0.20 max | 0.015 max | 24-26 | 0.15 max | 19-21 | 54.7 min |
| SS 310S | 0.08 max | 2 max | 1.0 max | 0.045 max | 0.030 max | 24 – 26 | 0.75 max | 19 – 21 | 53.095 min |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 7.9 g/cm3 | 1402 °C (2555 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 40 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
|---|---|---|---|---|---|---|---|
| SS 310 | 1.4841 | S31000 | SUS 310 | 310S24 | 20Ch25N20S2 | – | X15CrNi25-20 |
| SS 310S | 1.4845 | S31008 | SUS 310S | 310S16 | 20Ch23N18 | – | X8CrNi25-21 |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Fe |
|---|---|---|---|---|---|---|---|---|---|
| SS 310 | 0.015 max | 2 max | 0.15 max | 0.20 max | 0.015 max | 24-26 | 0.15 max | 19-21 | 54.7 min |
| SS 310S | 0.08 max | 2 max | 1.0 max | 0.045 max | 0.030 max | 24 – 26 | 0.75 max | 19 – 21 | 53.095 min |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 7.9 g/cm3 | 1402 °C (2555 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 40 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
|---|---|---|---|---|---|---|---|
| SS 316 | 1.4401 / 1.4436 | S31600 | SUS 316 | 316S31 / 316S33 | – | Z7CND17‐11‐02 | X5CrNiMo17-12-2 / X3CrNiMo17-13-3 |
| SS 316L | 1.4404 / 1.4435 | S31603 | SUS 316L | 316S11 / 316S13 | 03Ch17N14M3 / 03Ch17N14M2 | Z3CND17‐11‐02 / Z3CND18‐14‐03 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Fe |
|---|---|---|---|---|---|---|---|---|---|
| SS 316 | 0.015 max | 2 max | 1.0 max | 0.045 max | 0.030 max | 16.0-18.0 | 2.0-3.0 | 11.0-14.0 | 67.845 min |
SS 316L |
0.035 max | 2 max | 1.0 max | 0.045 max | 0.030 max | 16.0-18.0 | 2.0-3.0 | 10.0-14.0 | 68.89 min |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
|---|---|---|---|---|---|---|---|
| SS 316 | 1.4401 / 1.4436 | S31600 | SUS 316 | 316S31 / 316S33 | – | Z7CND17‐11‐02 | X5CrNiMo17-12-2 / X3CrNiMo17-13-3 |
| SS 316L | 1.4404 / 1.4435 | S31603 | SUS 316L | 316S11 / 316S13 | 03Ch17N14M3 / 03Ch17N14M2 | Z3CND17‐11‐02 / Z3CND18‐14‐03 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Fe |
|---|---|---|---|---|---|---|---|---|---|
| SS 316 | 0.015 max | 2 max | 1.0 max | 0.045 max | 0.030 max | 16.0-18.0 | 2.0-3.0 | 11.0-14.0 | 67.845 min |
SS 316L |
0.035 max | 2 max | 1.0 max | 0.045 max | 0.030 max | 16.0-18.0 | 2.0-3.0 | 10.0-14.0 | 68.89 min |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
| STANDARD | WERKSTOFF NR. | UNS |
|---|---|---|
| SS 304H | 1.4301 | S30409 |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N |
|---|---|---|---|---|---|---|---|---|---|
| SS 304H | 0.10 max | 2 max | 0.75 max | 0.045 max | 0.030 max | 18 – 20 | – | 8 – 10.5 | – |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 40 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
|---|---|---|---|---|---|---|---|
| SS 317 | 1.4449 | S31700 | SUS 317 | – | – | – | – |
| SS 317L | 1.4438 | S31703 | SUS 317L | – | – | – | – |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Fe |
|---|---|---|---|---|---|---|---|---|---|
| SS 317 | 0.08 max | 2 max | 1.0 max | 0.045 max | 0.030 max | 18 – 20 | 3.0-4.0 | 11.0-15.0 | 57.845 min |
| SS 317L | 0.035 max | 2 max | 1.0 max | 0.045 max | 0.030 max | 18 – 20 | 3.0-4.0 | 11.0-15.0 | 57.89 min |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
|---|---|---|---|---|---|---|---|
| SS 317 | 1.4449 | S31700 | SUS 317 | – | – | – | – |
| SS 317L | 1.4438 | S31703 | SUS 317L | – | – | – | – |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Fe |
|---|---|---|---|---|---|---|---|---|---|
| SS 317 | 0.08 max | 2 max | 1.0 max | 0.045 max | 0.030 max | 18 – 20 | 3.0-4.0 | 11.0-15.0 | 57.845 min |
| SS 317L | 0.035 max | 2 max | 1.0 max | 0.045 max | 0.030 max | 18 – 20 | 3.0-4.0 | 11.0-15.0 | 57.89 min |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | EN |
|---|---|---|---|---|
| SS 321 | 1.4541 | S32100 | SUS 321 | X6CrNiTi18-10 |
| SS 321H | 1.4878 | S32109 | SUS 321H | X12CrNiTi18-9 |
| Grade | C | Mn | Si | P | S | Cr | N | Ni | Ti |
|---|---|---|---|---|---|---|---|---|---|
| SS 321 | 0.08 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 17.00 – 19.00 | 0.10 max | 9.00 – 12.00 | 5(C+N) – 0.70 max |
| SS 321H | 0.04 – 0.10 | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 17.00 – 19.00 | 0.10 max | 9.00 – 12.00 | 4(C+N) – 0.70 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 8.0 g/cm3 | 1457 °C (2650 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | EN |
|---|---|---|---|---|
| SS 321 | 1.4541 | S32100 | SUS 321 | X6CrNiTi18-10 |
| SS 321H | 1.4878 | S32109 | SUS 321H | X12CrNiTi18-9 |
| Grade | C | Mn | Si | P | S | Cr | N | Ni | Ti |
|---|---|---|---|---|---|---|---|---|---|
| SS 321 | 0.08 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 17.00 – 19.00 | 0.10 max | 9.00 – 12.00 | 5(C+N) – 0.70 max |
| SS 321H | 0.04 – 0.10 | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 17.00 – 19.00 | 0.10 max | 9.00 – 12.00 | 4(C+N) – 0.70 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 8.0 g/cm3 | 1457 °C (2650 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
| STANDARD | UNS | WNR. | JIS | EN |
|---|---|---|---|---|
| SS 347 | S34700 | 1.4550 | SUS 347 | X6CrNiNb18-10 |
| SS 347H | S34709 | 1.4961 | SUS 347H | X6CrNiNb18-12 |
| C | Cr | Mn | Ni | P | S | Si | Cb/Ta | |
|---|---|---|---|---|---|---|---|---|
| 347 | 0.08 max | min: 17.0 max: 20.0 |
2.0 max | min: 9.0 max: 13.0 |
0.04 max | 0.30 max |
0.75 max |
min:10x C max: 1.0 |
| 347H | min: 0.04 max: 0.10 |
min: 17.0 max: 20.0 |
2.0 max | min: 9.0 max: 13.0 |
0.03 max | 0.30 max |
0.75 max |
min:10x C max: 1.0 |
| Grade | Tensile Strength ksi (MPa) min | Yield Strength 0.2% ksi offset ksi (MPa) min | Elongation (% in 50mm) min | Hardness (Brinell) MAX | Hardness (Rockwell B) MAX |
|---|---|---|---|---|---|
| 347/347H | 75 (515) |
30 (205) |
40 | 201 | 95 |
| STANDARD | UNS | WNR. | JIS | EN |
|---|---|---|---|---|
| SS 347 | S34700 | 1.4550 | SUS 347 | X6CrNiNb18-10 |
| SS 347H | S34709 | 1.4961 | SUS 347H | X6CrNiNb18-12 |
| C | Cr | Mn | Ni | P | S | Si | Cb/Ta | |
|---|---|---|---|---|---|---|---|---|
| 347 | 0.08 max | min: 17.0 max: 20.0 |
2.0 max | min: 9.0 max: 13.0 |
0.04 max | 0.30 max |
0.75 max |
min:10x C max: 1.0 |
| 347H | min: 0.04 max: 0.10 |
min: 17.0 max: 20.0 |
2.0 max | min: 9.0 max: 13.0 |
0.03 max | 0.30 max |
0.75 max |
min:10x C max: 1.0 |
| Grade | Tensile Strength ksi (MPa) min | Yield Strength 0.2% ksi offset ksi (MPa) min | Elongation (% in 50mm) min | Hardness (Brinell) MAX | Hardness (Rockwell B) MAX |
|---|---|---|---|---|---|
| 347/347H | 75 (515) |
30 (205) |
40 | 201 | 95 |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | KS | AFNOR | EN |
|---|---|---|---|---|---|---|---|
| SS 904L | 1.4539 | N08904 | SUS 904L | 904S13 | STS 317J5L | Z2 NCDU 25-20 | X1NiCrMoCu25-20-5 |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | Cu |
|---|---|---|---|---|---|---|---|---|---|
| SS 904L | 0.020 max | 2.00 max | 1.00 max | 0.040 max | 0.030 max | 19.00 – 23.00 | 4.00 – 5.00 max | 23.00 – 28.00 | 1.00 – 2.00 |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|
| 7.95 g/cm3 | 1350 °C (2460 °F) | Psi – 71000 , MPa – 490 | Psi – 32000 , MPa – 220 | 35 % |
| STANDARD | WERKSTOFF NR. | UNS | SAF |
| Super Duplex S32750 | 1.4410 | S32750 | 2507 |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | Fe |
| S32750 | 0.030 max | 1.20 max | 0.80 max | 0.035 max | 0.020 max | 24.00 – 26.00 | 3.00 – 5.00 | 6.00 – 8.00 | 0.24 – 0.32 | 58.095 min |
| UNS No | Grade | Proof Stress 0.2% (MPa) |
Tensile Strength (MPa) |
Elongation A5(%) |
Hardness Max | |
| HB | HRB | |||||
| S32750 | 2507 | 550 | 795 | 15 | 310 | 32* |
| STANDARD | WERKSTOFF NR. | UNS | SAF |
| Super Duplex S32760 | 1.4410 | S32760 | 2507 |
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | Fe |
| S32760 | 0.05 max | 1.00 max | 1.00 max | 0.030 max | 0.010 max | 24.00 – 26.00 | 3.00 – 4.00 | 6.00 – 8.00 | 0.20 – 0.30 | 57.61 min |
| Grades | Density (g/cm 3) | Density (lb/in 3) | Melting Point (°C) | Melting Point (°F) |
| S32760 | 7.8 | 0.281 | 1350 | 2460Standard |
| STANDARD | UNS | WNR. |
|---|---|---|
| Titanium Gr 1 | R50250 | 3.7025 |
| Grade | C | N | O | H | Ti | Fe |
|---|---|---|---|---|---|---|
| Titanium Gr 1 | .08 max | .03 max | .18 max | .015 max | Bal | .20 max |
| Grade | Tensile (ksi) | Yield Strength (ksi) | Elongation % |
|---|---|---|---|
| Titanium Gr 1 | 240 | 170 | 24 |
| STANDARD | UNS | WNR. |
|---|---|---|
| Titanium Gr 2 | R50400 | 3.7035 |
| Grade | C | N | O | H | Ti | Fe |
|---|---|---|---|---|---|---|
| Titanium Gr 2 | 0.10 max | 0.03 max | 0.25 max | 0.015 max | bal | 0.30 max |
| Grade | Tensile (ksi) | Yield Strength (ksi) | Hardness |
|---|---|---|---|
| Titanium Gr 2 | 50 | 40 | 14.9 |
| STANDARD | UNS | WNR. |
|---|---|---|
| Titanium Gr 5 | R56400 | 3.7165 |
| Grade | Ti | C | Fe | Al | V | O |
|---|---|---|---|---|---|---|
| Titanium Grade 5 | 90 min | – | 0.25 max | 6 min | 4 min | 0.02 max |
| lement | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|---|
| Titanium Gr. 5 | 4.43 g/cm3 | 1632 °C (2970 °F) | Psi – 138000 , MPa – 950 | Psi – 128000 , MPa – 880 | 14 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS |
| Hastelloy B2 | 2.4617 | N10665 | NW 0665 |
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| Hastelloy B2 | 0.02 max | 1.0 max | 0.1 max | 0.03 max | 1.0 max | Bal | 1.0 max | 2.0 max | 26 – 30 | 0.04 max |
| STANDARD | WERKSTOFF NR. | UNS |
| Hastelloy B3 | 2.4600 | N010675 |
| Grade | C | Mn | Si | Cu | Co | Ni | Cr | Fe | Mo | Ti |
| Hastelloy B3 | 0.01 max | 3.0 max | 0.10 max | 0.20 max | 3.0 max | 65.0 min | 1.5 max | 1.5 max | 28.5 max | 0.2 max |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Hastelloy B3 | 9.2 g/cm3 | 1370 °C (2550 °F) | Psi – 1,15,000 , MPa –760 | Psi – 52,000 , MPa – 350 | 40 % |
| STANDARD | WERKSTOFF NR. | UNS |
| Hastelloy C4 | 2.4610 | N06455 |
| Grade | Ni | Cr | Mo | Fe | C | Mn | Si | Co | Ti | S | P |
| Hastelloy C4 | Bal | 14.5-17.5 | 14.0-17.0 | Max 3.0 | Max 0.009 | Max 1.0 | Max 0.05 | Max 2.0 | Max 0.7 | Max 0.010 | Max 0.025 |
| Grade | Tensile Strength | Yield Strength RP0.2% | Elongation A5% | Mean Coefficient of Thermal Expansion |
| Hastelloy C4 | 690 N/mm² | 1335°C-1380°C | 275 N/mm² | 40% |
| STANDARD | WERKSTOFF NR. | UNS | JIS | EN |
| Hastelloy C22 | 2.4602 | N06022 | NW 6022 | NiCr21Mo14W |
| Grade | C | Mn | Si | Co | P | Fe | Mo | Ni | Cr | S | W | V |
| Hastelloy C22 | 0.010 max | 0.50 max | 0.08 max | 2.5 max | 0.02 max | 2 – 6 | 12.5 – 14.5 | Bal | 20 – 22.5 | 0.02 max | 2.5 – 3.5 | 0.35 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.69 g/cm3 | 1399 °C (2550 °F) | Psi – 1,00,000 , MPa – 690 | Psi – 45000 , MPa – 310 | 45% |
| STANDARD | WERKSTOFF NR. | UNS | JIS | EN |
| Hastelloy C276 | 2.4819 | N10276 | NW 0276 | NiMo16Cr15W |
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| C276 | 0.010 max | 1.00 max | 0.08 max | 0.03 max | 2.50 max | 50.99 min* | 14.50 – 16.50 | 4.00 – 7.00 | 15.00 – 17.00 | 0.04 max |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Hastelloy C276 | 8.89 g/cm3 | 1370 °C (2500 °F) | Psi – 1,15,000 , MPa – 790 | Psi – 52,000 , MPa – 355 | 40 % |
| STANDARD | WERKSTOFF NR. | UNS | AWS |
|---|---|---|---|
| Hastelloy C2000 | 2.4675 | N06200 | AWS 055 |
| Alloy (UNS) | Ni | Cr | Mo | W | Cu | Fe | Carbon |
|---|---|---|---|---|---|---|---|
| C2000 (N06200) | Bal | 22.00-24.00 | 15.00-17.00 | – | 1.30-1.90 | 3.00 max. | 0.010max. |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Hastelloy C2000 | 8.89 g/cm3 | 1065 °C (1950 °F) | 752 MPa (109.0 ksi) | 358 MPa (52.0 ksi) | 64 % |
| STANDARD | WERKSTOFF NR. | UNS |
| Hastelloy X | 2.4665 | N06002 |
| Grade | C | Mn | Si | Cu | Co | Ni | Cr | Fe | Mo | Ti |
| Hastelloy X | 0.05 - 0.15 | 1.0 max | 1.0 max | 0.50 max | 0.5 - 2.5 | Remainder | 20.5-23.0 | 17.0-20.0 | 8.0-10.0 | 0.15 max |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Hastelloy X | 8.22 g/cm³ | 1355°C | 655 MPa | 240 MPa | 35 % |
Incoloy 800 / 800H / 800HT Sheet & Plate Chemical Properties
| Grade | Ni | Fe | Cr | Cu | Ti | Al | C | Mn | S | Si |
| Incoloy 800 | 30.0-35.0 | 39.5 min | 19.0-23.0 | .75 max | .15-.60 | .15-.60 | .1 max | 1.5 max | .015 max | 1.0 max |
| Incoloy 800H | 30.0-35.0 | 39.5 min | 19.0-23.0 | .75 max | .15-.60 | .15-.60 | .05-.10 max | 1.5 max | .015 max | 1.0 max |
| Incoloy 800HT | 30.0-35.0 | 39.5 min | 19.0-23.0 | .75 max | .25-.60 | .85-1.20 | .06-.10 max | 1.5 max | .015 max | 1.0 max |
Incoloy 800 / 800H / 800HT Sheet & Plate Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.94 g/cm3 | 1350-1400 °C | Psi - 75,000 , MPa -520 | Psi - 30,000 , MPa - 205 | 30 - 35 % |
Incoloy 800 / 800H / 800HT Sheet & Plate Equivalent Grades
| STANDARD | UNS | WNR. | AFNOR | EN | JIS | BS | GOST | OR |
| Incoloy 800 | N08800 | 1.4876 | Z8NC32-21 | X10NiCrAlTi32-20 | NCF 800 | NA 15 | ЭИ670 | XH32T |
| Incoloy 800H | N08810 | 1.4958 | Z8NC32-21 | X10NiCrAlTi32-20 | NCF 800H | NA 15(H) | ЭИ670 | XH32T |
| Incoloy 800HT | N08811 | 1.4959 | - | X8NiCrAlTi32-21 | NCF 800HT | NA 15(HT) | ЭИ670 | XH32T |
| Grade | Ni | Fe | Cr | Cu | Ti | Al | C | Mn | S | Si |
| Incoloy 800 | 30.0-35.0 | 39.5 min | 19.0-23.0 | .75 max | .15-.60 | .15-.60 | .1 max | 1.5 max | .015 max | 1.0 max |
| Incoloy 800H | 30.0-35.0 | 39.5 min | 19.0-23.0 | .75 max | .15-.60 | .15-.60 | .05-.10 max | 1.5 max | .015 max | 1.0 max |
| Incoloy 800HT | 30.0-35.0 | 39.5 min | 19.0-23.0 | .75 max | .25-.60 | .85-1.20 | .06-.10 max | 1.5 max | .015 max | 1.0 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.94 g/cm3 | 1350-1400 °C | Psi - 75,000 , MPa -520 | Psi - 30,000 , MPa - 205 | 30 - 35 % |
| STANDARD | UNS | WNR. | AFNOR | EN | JIS | BS | GOST | OR |
| Incoloy 800 | N08800 | 1.4876 | Z8NC32-21 | X10NiCrAlTi32-20 | NCF 800 | NA 15 | ЭИ670 | XH32T |
| Incoloy 800H | N08810 | 1.4958 | Z8NC32-21 | X10NiCrAlTi32-20 | NCF 800H | NA 15(H) | ЭИ670 | XH32T |
| Incoloy 800HT | N08811 | 1.4959 | - | X8NiCrAlTi32-21 | NCF 800HT | NA 15(HT) | ЭИ670 | XH32T |
| Grade | Ni | Fe | Cr | Cu | Ti | Al | C | Mn | S | Si |
| Incoloy 800 | 30.0-35.0 | 39.5 min | 19.0-23.0 | .75 max | .15-.60 | .15-.60 | .1 max | 1.5 max | .015 max | 1.0 max |
| Incoloy 800H | 30.0-35.0 | 39.5 min | 19.0-23.0 | .75 max | .15-.60 | .15-.60 | .05-.10 max | 1.5 max | .015 max | 1.0 max |
| Incoloy 800HT | 30.0-35.0 | 39.5 min | 19.0-23.0 | .75 max | .25-.60 | .85-1.20 | .06-.10 max | 1.5 max | .015 max | 1.0 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.94 g/cm3 | 1350-1400 °C | Psi - 75,000 , MPa -520 | Psi - 30,000 , MPa - 205 | 30 - 35 % |
| STANDARD | UNS | WNR. | AFNOR | EN | JIS | BS | GOST | OR |
| Incoloy 800 | N08800 | 1.4876 | Z8NC32-21 | X10NiCrAlTi32-20 | NCF 800 | NA 15 | ЭИ670 | XH32T |
| Incoloy 800H | N08810 | 1.4958 | Z8NC32-21 | X10NiCrAlTi32-20 | NCF 800H | NA 15(H) | ЭИ670 | XH32T |
| Incoloy 800HT | N08811 | 1.4959 | - | X8NiCrAlTi32-21 | NCF 800HT | NA 15(HT) | ЭИ670 | XH32T |
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| Inconel 600 | 0.15 max | 1.00 max | 0.50 max | 0.015max | 0.50 max | 6.00 – 10.00 | 72.00 min | 14.00 – 17.00 |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 600 | 8.47 g/cm3 | 1413 °C (2580 °F) | Psi – 95,000 , MPa – 655 | Psi – 45,000 , MPa – 310 | 40 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Inconel 600 | 2.4816 | N06600 | NCF 600 | NA 13 | МНЖМц 28-2,5-1,5 | NC15FE11M | NiCr15Fe |
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| 601 | 0.10 max | 1.0 max | 0.5 max | 0.015 max | 1.0 max | Balance | 58.0 – 63.0 | 21.0 – 25.0 |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 601 | 8.1 g/cm3 | 1411 °C (2571 °F) | Psi – 80,000 , MPa – 550 | Psi – 30,000 , MPa – 205 | 30 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| 601 | 2.4851 | N06601 | NCF 601 | NA 49 | XH60BT | NC23FeA | NiCr23Fe |
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| 625 | 0.10 max | 0.50 max | 0.50 max | 0.015 max | - | 5.0 max | 58.0 min | 20.0 - 23.0 |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 625 | 8.4 g/cm3 | 1350 °C (2460 °F) | Psi – 1,35,000 , MPa – 930 | Psi – 75,000 , MPa – 705 | 42.5 % |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| 625 | 2.4856 | N06625 | NCF 625 | NA 21 | ХН75МБТЮ | NC22DNB4M | NiCr22Mo9Nb |
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| 718 | 0.08 max | 0.35 max | 0.35 max | 0.015 max | 0.30 max | - | 50.00 - 55.00 | 17.00 - 21.00 |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) |
| 8.2 g/cm3 | 1350 °C (2460 °F) | Psi – 1,35,000 , MPa – 930 | Psi – 75,000 , MPa – 482 | 45 % |
| STANDARD | WERKSTOFF NR. | UNS |
| 718 | 2.4668 | N07718 |
| Grade | Common Name | C% | Mn% | Si% | P% | S% | Cr% | Ni% | Mo% | N% |
| 2205 | S31803 | 0.030 | 2.00 | 1.00 | 0.030 | 0.020 | 21.0-23.0 | 4.5-6.5 | 2.5-3.5 | 0.08-0.20 |
| 2205 | S32205 | 0.030 | 2.00 | 1.00 | 0.030 | 0.020 | 22.0-23.0 | 4.5-6.5 | 3.0-3.5 | 0.14-0.20 |
| Tensile strength | 620MPa min | Density | 7,805kg/m3 |
| Yield strength | 450MPa mi | Elastic modulus | 200GPa |
| STANDARD | WNR. |
| Duplex S31803 / S32205 | 1.4462 |
| Grade | Common Name | C% | Mn% | Si% | P% | S% | Cr% | Ni% | Mo% | N% |
| 2205 | S31803 | 0.030 | 2.00 | 1.00 | 0.030 | 0.020 | 21.0-23.0 | 4.5-6.5 | 2.5-3.5 | 0.08-0.20 |
| 2205 | S32205 | 0.030 | 2.00 | 1.00 | 0.030 | 0.020 | 22.0-23.0 | 4.5-6.5 | 3.0-3.5 | 0.14-0.20 |
| Tensile strength | 620MPa min | Density | 7,805kg/m3 |
| Yield strength | 450MPa mi | Elastic modulus | 200GPa |
| STANDARD | WNR. |
| Duplex S31803 / S32205 | 1.4462 |
| C | Cr | Ni | Mo | N | Others |
| 0.020 | 25 | 7 | 4.0 | .27 | S=0.001 |
| Ultimate Tensile Strength, ksi | 116 min. |
| 0.2% Offset Yield Strength 0.2%, ksi | 80 min. |
| 0.1% Offset Yield Strength 0.2%, ksi | 91 min. |
| Elongation in 2 inches, % | 15 min. |
| Hardness Rockwell C | 32 max. |
| Impact Energy, ft.-lbs. | 74 min. |
| STANDARD | WNR. |
| Super Duplex S32750 / S32760 | 1.4410 |
| C | Cr | Ni | Mo | N | Others |
| 0.020 | 25 | 7 | 4.0 | .27 | S=0.001 |
| Ultimate Tensile Strength, ksi | 116 min. |
| 0.2% Offset Yield Strength 0.2%, ksi | 80 min. |
| 0.1% Offset Yield Strength 0.2%, ksi | 91 min. |
| Elongation in 2 inches, % | 15 min. |
| Hardness Rockwell C | 32 max. |
| Impact Energy, ft.-lbs. | 74 min. |
| STANDARD | WNR. |
| Super Duplex S32750 / S32760 | 1.4410 |
| C | Fe | H | N | O | Ti |
| 0.1 | 0.2 | 0.015 | 0.03 | 0.18 | 99.5 |
| Grade | Tensile (ksi) | Yield Strength (ksi) | Elongation % |
| Titanium Gr 1 | 240 | 170 | 24 |
| STANDARD | UNS | WNR. |
| Titanium GR 1 | R50250 | 3.7025 |
| C | Fe | H | N | O | Ti |
| 0.1 | 0.3 | 0.015 | 0.03 | 0.25 | 99.2 |
| Grade | Tensile (ksi) | Yield Strength (ksi) | Hardness |
| Titanium Gr 2 | 50 | 40 | 14.9 |
| STANDARD | UNS | WNR. |
| Titanium GR 2 | R50400 | 3.7035 |
| Al | Fe | O | Ti | V |
| 6 | 0.25 | 0.2 | 90 | 4 |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Titanium Gr. 5 | 4.43 g/cm3 | 1632 °C (2970 °F) | Psi – 138000 , MPa – 950 | Psi – 128000 , MPa – 880 | 14 % |
| STANDARD | UNS | WNR. |
| Titanium GR 5 | R56400 | 3.7165 |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Monel 400 | 2.4360 | N04400 | NW 4400 | NA 13 | МНЖМц 28-2,5-1,5 | NU-30M | NiCu30Fe |
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Monel 400 | 0.30 max | 2.00 max | 0.50 max | 0.024 max | 28.00 – 34.00 | 2.50 max | 63.00 min |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Monel 400 | 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 80,000 , MPa – 550 | Psi – 35,000 , MPa – 240 | 40 % |
| STANDARD | UNS |
| Monel R405 | N04405 |
| Designation | Ni% | C% | Ti% | Ai% | Co% | Cr% | V% | W% | Mo% | Cu% | Nb/Cb Ta% | Fe% | Sonstige Autres-Other % |
| Alloy R 405 | 66.0 | 0.15 | - | - | - | - | - | - | - | 31.0 | - | 1.2 | Mn 1.0; S 0.04 |
| Mechanical Analysis | |
| Tensile strength, Ultimate | 550 Mpa |
| Tensile strength, Yield | 240 Mpa |
| Elongation at Break | 48% |
| STANDARD | WERKSTOFF NR. | UNS |
| Monel K500 | 2.4375 | N05500 |
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Monel K500 | 0.25 max | 1.5 max | 0.5 max | 0.010 max | 27.00 – 33.00 | 0.5 – 2 | 63.00 min |
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Monel K500 | 8.44 g/cm3 | 1350 °C (2460 °F) | Psi – 160000 , MPa – 1100 | Psi – 115000 , MPa – 790 | 20 % |
| Grade | C | Mn | Si | S | Cu | Ni | Cr | Fe | Mo | P |
| Alloy 20 | 0.07 max | 2.00 max | 1.00 max | 0.035 max | 3.0-4.0 | 32.0-38.0 | 19.0-21.0 | 29.85 min* | 2.0-3.0 | 0.045 max |
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.1 g/cm3 | 1443 °C (2430 °F) | Psi -80,000, MPa -551 | Psi – 35,000, MPa – 241 | 30% |
| STANDARD | WERKSTOFF NR. | UNS | AFNOR | EN |
| Alloy 20 | 2.4660 | N08020 | Z2NCUD31-20AZ | NiCr20CuMo |
| Grade | Cr | Ni | Mo | C | W | Cu | N | Mn | Si | P | S | |
| Zeron 100 | 24.0-26.0 | 6.0-8.0 | 3.0-4.0 | 0.030 Max | 0.5-1.0 | 0.50-1.0 | 0.2-0.3 | 1.00 Max | 1.0 Max | 0.03 Max | 0.01 Max |
| Grades | Alloy Zeron 100 Tensile Strength, ksi | .2% Yield Strength, ksi | % Elongation in 50mm | Hardness Max. |
| Zeron 100 | 109 | 80 | 25 | 28 HRC |
| STANDARD | WERKSTOFF NR. | UNS |
| Zeron 100 | 1.4501 | S32760 |
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Nickel 200 | 0.15 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
| Nickel 201 | 0.02 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
| Grade | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Nickel 200 | 8.9 g/cm3 | 1446 °C (2635 °F) | Psi – 67000 , MPa – 462 | Psi – 21500 , MPa – 148 | 45 % |
| Nickel 201 | 8.9 g/cm3 | 1446 °C (2635 °F) | Psi – 67000 , MPa – 462 | Psi – 21500 , MPa – 148 | 45 % |
| STANDARD | UNS | WNR. | JIS | EN |
| Nickel 200 | N02200 | 2.4066 | NW 2200 | Ni 99.2 |
| Nickel 201 | N02201 | 2.4068 | NW 2201 | LC-Ni 99 |
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Nickel 200 | 0.15 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
| Nickel 201 | 0.02 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
| Grade | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Nickel 200 | 8.9 g/cm3 | 1446 °C (2635 °F) | Psi – 67000 , MPa – 462 | Psi – 21500 , MPa – 148 | 45 % |
| Nickel 201 | 8.9 g/cm3 | 1446 °C (2635 °F) | Psi – 67000 , MPa – 462 | Psi – 21500 , MPa – 148 | 45 % |
| STANDARD | UNS | WNR. | JIS | EN |
| Nickel 200 | N02200 | 2.4066 | NW 2200 | Ni 99.2 |
| Nickel 201 | N02201 | 2.4068 | NW 2201 | LC-Ni 99 |
| Grade | Ni | Cr | Fe | P | Cu | Al | Ti | C | Mn | Si | |
| Nimonic 75 | Bal. | 19-22 | Max 1.0 | Max 0.015 | Max 0.2 | Max 0.15 | 0.15-0.35 | Max 0.12 | Max 0.70 | Max 0.80 |
| Grade Nimonic 75 |
Tensile strength(annealed) | Yield strength(annealed) | Elongation at Break | Modulus of Elasticity |
| Metric | 750 MPa | 275 MPa | 42% | 206 GPa |
| Imperial | 109 ksi | 40 ksi | 42% | 29878 ksi |
| STANDARD | WERKSTOFF NR. | UNS |
| Nimonic 75 | 2.4951 | N06075 |
| Grade | Al | B | C | Cr | Co | Cu | Fe | Mn | Ni | P | Si | S |
| Nimonic 80A | 1 – 1.8 | 0.008 max | 0.1 max | 18 – 21 | 0.2 max | 0.2 max | 3 max | 1 max | Balance | 0.045 max | 1 max | 0.015 max |
| Grade | Condition | Ultimate Tensile Strength MPA | Yield Strength MPA | Elongation on 4D (min) | Hardness min |
| Nimonic 80A | Solution Annealed & Precipatation Treated (aged) | 994 | 616 | 20 | 300 HV |
| STANDARD | WERKSTOFF NR. | UNS |
| Nimonic 80A | 2.4952 | N07080 |
| Grade | Ni | Co | Cr | Mo | Ti | Fe | Mn | Al | Si | Cu | C | B | S |
| Nimonic 263 | 49 | 19-21 | 19-21 | 5.60-6.10 | 1.90-2.40 | 0.70 | 0.60 | 0.60 | 0.40 | 0.20 | 0.040 – 0.080 | 0.0050 | 0.0070 |
| Grade | Material Sheet |
Temperature °C | Yield Strength 0.2 % (MPa) | Tensile Strength (MPa) | Elongation (%) | Hardness HV |
| Nimonic 263 | Nimonic 263 Sheet Solution Treated (AMS 5872 / BS HR206) |
RT | – | – | – | 22.5 max |
| Nimonic 263 Sheet Heat Treated (AMS 5872 / BS HR206 |
RT | 580 (typical) | 973 (typical) | 39 – | – | |
| Nimonic 263 Sheet Heat Treated (AMS 5872 / BS HR206 |
780 | 403 (min) | 541 (min) | 9 | – |
| STANDARD | WERKSTOFF NR. | UNS |
| Nimonic 263 | 2.4650 | N07263 |