Company Information
Ask for more detail from the seller
Contact Supplier| Material | Tensile temper strength elongation N/mm% on 50mm | Vickers Hardness | Complies with or falls within ISO | JIS | |
|---|---|---|---|---|---|
| 'O' | 210 min 35 min | 55 max | |||
| Electrolytic Tough | M | 210 min 35 min | 65 max | Cu ETP | H 3100 |
| Pitch H.C Copper | ½ H | 210 min 10 min | 70 to 95 | ISO : 1337 | C 1100 |
| H | 290 min | 90 Min | |||
| 'O' | 210 min 35 min | 55 max | |||
| Phosphorous | M | 210 min 35 min | 65 max | Cu DHP | H 3100 |
| Deoxidised Copper | ½ H | 240 min 10 min | 70 to 95 | ISO : 1337 | C 1220 |
| H | 290 min | 90 Min |
| Material | Normal Composition | Nearest Relevant Composition Specification | ||
|---|---|---|---|---|
| Electrolytic tough Pitch H.C. Copper | 99.92% Min. Cu | C 101 | Cu ETP 1337 | H 3100 C 2100 |
| Phosphorous Deoxidized Copper ( DONA) | 99.92% Min. Cu P.0.0134-0.05 | C 106 | Cu DHP 1337 | H 3100 C 122 |